摘要:叙述了对Cr12钢渗硼拉深凹模的选材及热处理,模具的渗硼工艺是950℃保温5h,出炉空冷,200℃回火1.5h。使用Cr12钢渗硼拉深凹模后在提高生产效率、节电和降低废品率方面都有较明显的效果。
注:因版权方要求,不能公开全文,如需全文,请咨询杂志社
热门期刊服务
Acta Pharmacologica Sinica Journal of Semiconductors Journal of Genetics and Genomics Hepatobiliary Pancreatic Diseases International Journal of Systems Engineering and Electronics Hepatobiliary Pancreatic Diseases International China World Economy Chinese Optics Letters Nuclear Science and Techniques Acta Metallurgica Sinica ComputerDIY玩脑者 Journal of Hydrodynamics